Hi everyone, as always, I am very exciting about reading the progress of our projects, therefore I want to continue sharing with yall a little more about mine. Last time I left at the conclusion that:
“TPO is most suitable photo-initiator to apply to PEGDA + PTC polymer, so is 369 for PEGDA+ TET.”
After conducting further experimentation and analysis such as microscopic observations and contact angle test (shown below),
PEGDA + PTC + TPO (smaller contact angle ∠20 or smaller)
PEGDA+ TET + 369 (bigger contact angle ∠20 or higher)
we concluded that PEGDA+PTC+TPO is the most suitable combination to disperse CNT, and thus to make the material for the development of the ink.
We will be conducting further research to determine proper concentration (maximum), and will definitely keep you guys updated with FINAL results.
Truly hope everyone has an excellent and productive week, as we get closer to final weeks. SI SE PUEDE!